Iron-based nanocrystalline magnetic powder core
- Model
- Brand
- Price
Main parameters: the Curie temperature Tc (℃) : 500 ℃ or higher saturated magnetic induction intensity of Bs (T) : 1.2 T effective permeability mu e: mu e26 - mu e125 Loss: Loss of 190 mw/cm3 @ 100 KHZ, 500 gs (60 mu e) is mainly used: high-power switching power supply transformer/filter inductor/transformer High - frequency big power switching power supply transformer/filter inductance/tra
GDLN系列磁粉芯是由Fe-Si-B-Nb-Cu合金组成,具有优良的软磁性能,低损耗、低矫顽力,较高的饱和磁感应强度和良好的频率特性和温度特性,同时具有很小的磁致伸缩系数。
主要参数: | 主要应用: |
·居里温度Tc(℃):≥500℃ | ·大功率开关电源变压器/滤波电感/互感器 |
·饱和磁感应强度Bs(T):1.2T | ·PFC电感 |
·有效磁导率μe:μe26—μe125 | ·DC-DC变换器DC-DC |
·损耗Loss:190mw/cm3 @ 100KHz,500Gs(μe 60) | ·一般工业用电的输出电感 |