Silicon iron magnetic powder core
- Model
- Brand
- Price
Main parameters: the Curie temperature Tc (℃) : 500 ℃ or higher saturated magnetic induction intensity of Bs (T) : 1.5 T effective permeability mu e: mu e26 125 - mu e Loss: Loss of 700 mw/cm3 @ 50 KHZ, 1000 gs main applications: power accompanying vibration inductor, choke coil Switch power modulation inductancePFC PFC inductor inductance and Output filter inductance Output filter inductance of Pulse transformer Pulse T
GDLF系列粉芯是由Fe-Si合金粉构成,可取代铁粉芯及部分High-Flux 粉芯。铁硅磁粉芯具有高饱和磁感应强度,损耗明显比铁粉芯低,近零的磁感应强度;同时具有优良的直流偏置性能,特别推荐使用在大电流的应用条件。
主要参数: 主要应用
·居里温度 Tc(℃):≥500℃ ·功率偕振电感器、扼流圈
·饱和磁感应强度Bs(T):1.5T ·PFC电感
·有效磁导率μe:μe26--μe 125 ·输出滤波电感
·损耗Loss:700mw/cm3 @ 50KHz,1000Gs ·脉冲变压器